Highly Li-ion conductive 78Li 2 S-22P 2 S 5 glass-ceramic electrolytes were prepared by simple heat treatment of the glass phase obtained via mechanical ball milling. A high ionic conductivity of ∼1.78 × 10 –3 S cm –1 is achieved at room temperature and is attributed to the formation of a crystalline phase of high lithium-ion conduction. All-solid-state lithium-ion batteries based on these glass-ceramic electrolytes are assembled by using Li 2 S nanoparticles or low-cost commercially available FeS 2 as active cathode materials and Li–In alloys as anode. A high discharge capacity of 535 mAh g –1 is achieved after at least 50 cycles for the all-solid-state cells with Li 2 S as cathode materials, suggesting a rather high capacity retention of 97.4%. Even for the cells using low-cost FeS 2 as cathode materials, same high discharge capacity of 560 mAh g –1 is also achieved after at least 50 cycles. Moreover, the Coulombic efficiency remain at ∼99% for these all-solid-state cells during the charge–discharge cycles.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2017) studied this question.
Synapse has enriched one closely related paper. Consider it for comparative context: