Woody yard waste with high lignin content (22% of dry matter (DM)) was subjected to wet oxidation pre‐treatment for subsequent enzymatic conversion and fermentation. The effects of temperature (185–200 °C), oxygen pressure (3–12 bar) and addition of sodium carbonate (0–3.3 g per 100 g DM biomass) on enzymatic cellulose and hemicellulose (xylan) convertibility were studied. The enzymatic cellulose conversion was highest after wet oxidation for 15 min at 185 °C with addition of 12 bars of oxygen and 3.3 g Na2CO3 per 100 g waste. At 25 FPU (filter paper unit) cellulase g−1 DM added, 58–67% and 80–83% of the cellulose and hemicellulose contained in the waste were converted into monomeric sugars. The cellulose conversion efficiency during a simultaneous saccharification and fermentation (SSF) assay at 10% DM was 79% for the highest enzyme loading (25 FPU g−1 DM) while 69% conversion efficiency was still reached at 15 FPU g−1 DM. Total carbohydrate recoveries were high (91–100% for cellulose and 72–100% for hemicellulose) and up to 49% of the original lignin and 79% of the hemicellulose could be solubilized during wet oxidation treatment and converted into carboxylic acids mainly (total carboxylic acids = 3.1–7.4% on DM basis).
No takes yet. Share an insight, caveat, or question.
Lissens et al. (2004) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: