A novel polymerizable phospholipid with conjugated diene groups at the hydrocarbon chain ends, 1,2‐bis(11,13‐tetradecadienoyl)‐sn‐glycero‐3‐phosphocholine (7), was synthesized. This phospholipid gives liposomes which can be readily polymerized upon γ‐and UV‐irradiation. The conversion is up to 95% within 10 h at 60°C or within 3 days at room temperature. According to light scattering, 31P NMR and electron microscopy, the polymerized liposomes are detergent‐resistent and maintain their structure under ultrasonic treatment and in organic solvent media.