We report on the synthesis of polycrystalline thin films of PbZr0.3Ti0.7O3 (PZT) by the so-called chemical solution deposition technique. The thin films were deposited on Pt∕Ti∕SiO2∕Si substrates by the spin-coating method, and were heat treateded at 700°C in air and under several oxygen pressures (10