The effect of uniaxial tensile strain on the shear mode (C mode) and layer breathing mode (LB mode) of few layers MoS 2 were studied. The C mode is doubly degenerated into two sub-peaks as applied strain increases. No measurable Raman shift for the LB mode is observed, while its Raman intensity decreases gradually as the strain increases. In addition, the C and LB modes exhibit distinguished thickness dependence. The C mode shows a clear blueshift as the strain increases, while the LB mode is softened in the process. Moreover, the evolution of C mode with thickness follows an enhanced linear-chain model plus a linear component very well. It implies that the C mode is a better thickness navigator as compared to the L mode.