This paper reports the preparation of cobalt silicate (Co 2 SiO 4 , CSO) first by a cost-effective and simple sonochemical route, followed by the fabrication of Co 2 SiO 4 /g-C 3 N 4 (CSO/CN) nanocomposites with different mass ratios by ultrasonic-assisted co-precipitation. We have investigated the photocatalytic performance of Co 2 SiO 4 , g-C 3 N 4 , and different Co 2 SiO 4 /g-C 3 N 4 nanocomposites for the degradation of eriochrome black T (EB). This initial instance of CSO integrated with CN demonstrates a superior function in photocatalysis. The outcomes indicated that multiple parameters affected effectiveness, including the amount of CSO, catalyst, and EB. As a result, CSO/CN with a weight ratio of 0.1:1 is the most efficient, which means that 0.07 g of CSO/CN (0.1:1) is capable of degrading 90.0% of 10 ppm EB. Photodegradation reactions were demonstrated by the scavenger tests to be largely influenced by superoxide radicals. The kinetic investigation showed that a bigger rate constant ( k = 0.0166 min ‒1 ) leads to higher efficiency (90.0%). The combination of CSO and CN as composites shows great potential for efficient photocatalytic dye degradation applications. Advanced materials for environmental treatment procedures may be developed as a result of further research and development in this field.
No takes yet. Share an insight, caveat, or question.
Hosseini et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: