Fiber‐structure‐development in the poly(ethylene terephthalate) fiber drawing process was investigated with online measurements of wide‐angle and small‐angle X‐ray scattering with both a high‐luminance X‐ray source and a CO2‐laser‐heated drawing system. The intensity profile of the transmitted X‐ray confirmed the location of the neck‐drawing point. The diffraction images had a time resolution of several milliseconds, and this still left much room for improvement. Crystal diffraction appeared in the wide‐angle X‐ray images almost instantaneously about 20 ms after necking, whereas a four‐point small‐angle X‐ray scattering pattern appeared immediately after necking. With the elapse of time after necking, the four‐point scattering pattern changed into a meridional two‐point shape.