Boron-doped polycrystalline diamond (BDD) and highly oriented pyrolytic graphite (HOPG) surfaces were exposed to low pressure hydrogen plasma. The relative yields of surface-produced H− ions were measured by an energy analyser quadrupole mass spectrometer. The highest H− yield was obtained at 400 °C for a BDD surface and at room temperature for an HOPG surface. At low ion bombardment energy, the maximum yield on a BDD surface is about 5 times higher than that on an HOPG surface, which has been the best carbon material so far for surface production of H− ions in caesium-free plasma. Raman measurements revealed surface modifications after plasma exposure.