Aromatic polyamides (aramids) having pendant t‐butyl group were synthesized by the direct polycondensation of 5‐t‐butylisophthalic acid with various aromatic diamines in N‐methyl‐2‐pyrrolidone (NMP) using triphenyl phosphite and pyridine as condensing agents. The aramids having inherent viscosities of 0.6–2.4 dL/g were obtained in quantitative yields. These polymers were readily soluble in various solvents such as NMP,N,N‐dimethylacetamide, dimethyl sulfoxide, and pyridine, and gave transparent, tough and flexible films by casting from the NMP solutions. The aramids had glass transition temperatures between 250 and 330°C, and started to lose weight around 350°C, with 10% weight loss being recorded at about 450°C in air.