Dimensional and phase changes of four candidate oxygen carrier materials for chemical looping combustion are investigated by dilatometry and high-temperature X-ray diffraction during four redox cycles. NiO/Ni 2 AlO 4 does not exhibit significant dimensional changes during cycling, and it is shown that the support material also contributes to the oxygen carrying capacity. CaMn 0.875 Ti 0.125 O 3 exhibited good chemical stability and small dimensional changes upon redox cycling. Cu 0.95 Fe 1.05 AlO 4 showed a one-dimensional expansion of 9% after the experiments, and significant phase changes were seen. The complex set of reactions occurring during redox cycling of ilmenite (FeTiO 3 ) was shown to be accompanied by dimensional changes, giving non-steady dimensional changes during the oxidation and reduction steps.