Particular aspects concerning the magnetoelastic behavior of an Fe-rich glass-covered amorphous ferromagnetic microwire (diameter about 20 /spl mu/m) are reported in both the as-prepared state and after various heat treatments. The main feature of such behavior is that related with the bistable behavior exhibited by the microwire. The magnetization process takes place by a single and large Barkhausen jump at a given applied field. For the as-prepared material, the value of this switching field (H*/spl ap/112 Am/sup -1/) is about one order of magnitude larger than that reported for Fe-rich amorphous wires with a diameter of about 125 /spl mu/m (H*/spl ap/8 Am/sup -1/). The effect of the thermal treatment as well as the stress dependence of H* for as-obtained and treated microwire are also reported and discussed in terms of the stress distribution within the microwire.
No takes yet. Share an insight, caveat, or question.
González et al. (1997) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: