The application of porous hydroxyapatite-collagen (HAp-Collagen) as a bone tissue engineering scaffold is hindered by two main problems: its high cost and low initial strength. As a native 3-dimenssional collagen framework, purified porcine acellular dermal matrix (PADM) has been successfully used as a skin tissue engineering scaffold. Here we report its application as a matrix for the preparation of HAp to produce a bone tissue scaffold through a biomimetic chemical process. The HAp-PADM scaffold has two-level pore structure, with large channels (∼100 μm in diameter) inherited from the purified PADM microstructure and small pores (<100 nm in diameter) formed by self-assembled HAp on the channel surfaces. The obtained HAp-PADM scaffold (S15D) has a compressive elastic modulus as high as 600 kPa. The presence of HAp in sample S15D reduces the degradation rate of PADM in collagenase solution at 37°C. After 7 day culture of MC3T3-E1 pre-osteroblasts, MTT data show no statistically significant difference on pure PADM framework and HAp-PADM scaffold (p > 0.05). Because of its high strength and nontoxicity, its simple preparation method, and designable and tailorable properties, the HAp-PADM scaffold is expected to have great potential applications in medical treatment of bone defects.
No takes yet. Share an insight, caveat, or question.
Zhao et al. (2010) studied this question.