Single crystals of disordered NaLa(WO4)2 and NaLa(MoO4)2 doped with Yb3+ are grown by the Czochralski method from the melt. Continuous‐wave laser operation with Ti:sapphire laser pumping is demonstrated at room temperature without special cooling. Tunability from 1017 to 1057 nm and from 1015 to 1053 nm is achieved for Yb:NaLa(WO4)2 and Yb:NaLa(MoO4)2, respectively. A maximum output power of 205 mW is obtained with Yb:NaLa(WO4)2. (© 2005 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)