Ti 3 Si(Al)C 2 films were electrophoretically deposited at 3 V on indium‐tin‐oxide (ITO) conductive glass from Ti 3 Si(Al)C 2 aqueous suspension with 1 vol% solid loading at pH 9 in the absence of any dispersant. The surface morphology, cross section microstructure, and preferred orientation of the films were investigated by scanning electron microscopy and X‐ray diffraction. The as‐deposited Ti 3 Si(Al)C 2 films exhibited (00 l ) preferred orientation and the thickness can be controlled by the deposition–drying–deposition method. These results demonstrate that electrophoretic deposition is a simple and feasible method to prepare MAX‐phases green films at room temperature.