Thin diamond films were deposited on silicon, MgO, fused silica, and soda lime silica glass at low temperature (the lowest temperature ∼365 °C) by microwave plasma-enhanced chemical vapor deposition. The films were identified as diamond by Raman spectroscopy. A Raman peak shift of several wave numbers to either lower or higher wave numbers due to the strain of the film is also observed. The film deposited on glass is highly transparent. The fine faceted crystals in the film are shown in scanning electron microscope micrographs.