The purpose of this study was to investigate the effect of a 4-MET- and 10-MDP-based primer on the bond strength of two resin cements (SuperBond C&B, Sun Medical; Panavia Fluoro Cement, Kuraray) to titanium (Ti). Ti plates were treated with six experimental primers consisting of, respectively, 10-MDP and 4-MET in concentrations of 0.1, 1 and 10wt%, or were kept untreated (control). The highest tensile bond strength of Panavia Fluoro Cement to Ti was obtained when the Ti surface was pre-treated with 10wt% 10-MDP and was significantly higher than that when a lower concentrated 10-MDP-based primer or any 4-MET-based primer was used. On the contrary, no significant difference in tensile bond strength of SuperBond C&B was found for the untreated and six pre-treated Ti surfaces, although pre-treatment with each 10-MDP-based primer resulted in a higher tensile bond strength as compared to any 4-MET pre-treatment. Altogether, the data obtained strongly suggest that 10-MDP is effective to improve the adhesive performance of resin to titanium.
No takes yet. Share an insight, caveat, or question.
Tsuchimoto et al. (2006) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: