Metal cluster cations are produced in a laser vaporization source, size selected in the gas phase by an electrostatic quadrupole deflector, and deposited without coalescence on carbon coated electron microscopy grids for further observation. For platinum clusters, a transition from spherical to strongly ramified shapes is observed when the cluster size increases beyond a critical diameter dc of about 2.50.3em0exnm. In ramified structures, the branch width is almost independent of the size and of the order of dc. This study shows evidence of the role of coagulation in the kinetics of growth and of the quenching of particle coalescence above the critical size. The results are discussed in the framework of previous models developed in aerosol and thin film growth experiments. A comparison with indium and gold clusters confirms that the border size at the transition from coalescence to ramification depends on the thermodynamic properties of the element.
No takes yet. Share an insight, caveat, or question.
Alayan et al. (2006) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: