The electrochemical behavior of zirconium on a liquid cadmium electrode was studied in LiCl–KCl melts containing 1.0 mol % ZrCl 4 at 773 K. In a cyclic voltammogram of the liquid cadmium electrode, a cathodic peak was observed at around − 1.0 V (vs Ag + / Ag ) as well as at − 1.05 V attributed to zirconium metal deposition. Because the deposit obtained by potentiostatic electrolysis at − 1.03 V was confirmed to be Cd 2 Zr from X-ray diffraction analysis, the cathodic peak at − 1.0 V corresponded to Cd 2 Zr formation. The open-circut-potential of the liquid cadmium electrode with Cd 2 Zr was measured to calculate thermodynamic properties such as relative partial molar Gibbs energies of zirconium in Cd 2 Zr . The quantity of zirconium recovered in the liquid cadmium electrode by the potentiostatic electrolysis at − 1.03 V was measured by inductively coupled plasma-atomic emission spectroscopy. The result indicated 96 % of the zirconium recovery efficiency, which was defined as the quantity of electricity corresponding to the recovered zirconium divided by the total quantity of passed electricity.
No takes yet. Share an insight, caveat, or question.
Murakami et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: