A simple procedure to elaborate robust ultraflat gold surface without clean room facilities is presented. Self-assembled 3-mercaptopropytriethoxysilane (MPTMS) on silicon was used as a buffer layer on which gold was sputtered using a common sputter-coating apparatus. The optimization of the sample position into the chamber of the sputtering machine yielded the formation of a thin (approximately 8 nm) gold layer. The characterization of the resulting gold surface (i.e., AFM, X-ray reflectivity, and diffraction) has demonstrated its high smoothness (<0.7 nm) over a large scale with a preferred (111) orientation. The robustness of the substrate toward organic solvents and thermal treatment was also tested. The ability of these surfaces to be used as substrates for high-resolution surface modification was confirmed by functionalizing the gold surface using the dip pen nanolithography process.
No takes yet. Share an insight, caveat, or question.
Pattier et al. (2008) studied this question.
Synapse has enriched 4 closely related papers on similar clinical questions. Consider them for comparative context: