The effects of immediate dentin sealing (IDS) applications on the bonding of computer-aided design/computer-aided manufacturing (CAD/CAM) ceramic onlay restorations after cyclic loading were examined. Standardized mesial-distal-occlusal-palatal cavities in 32 extracted human molars were prepared. The cavities were divided into four groups: those receiving thin-layered (T), slope-shaped (S), and base-shaped (B) sealing, and the non-sealing group (N) as a control. The intra-cavity dentin walls of the T, S, and B groups were sealed with an all-in-one adhesive and a flowable composite. All cavities were scanned; hence, CAD/CAM onlays were fabricated using ceramic blocks and bonded with a resin cement system. Cyclic loading was applied and the microtensile bond strength (μ-TBS) was measured. It was found that IDS application improved not only the μ-TBS, but also the bonding reliability and durability of the CAD/CAM restoration. In particular, the S restoration exhibited the highest-performance as regards both robust bond strength and stable bonding.
No takes yet. Share an insight, caveat, or question.
Murata et al. (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: