Mesoporous silica materials with hydroxyphosphatoethyl pendant groups (POH-MS) were obtained by a two-step process: (1) block copolymer Pluronic P123-templated synthesis of mesoporous silica with diethylphosphatoethyl groups (DP-MS) by co-condensation of diethylphosphatoethyl triethoxysilane (DPTS) and tetraethylorthosilicate (TEOS) under acidic conditions and (2) conversion of diethylphosphatoethyl into hydroxyphosphatoethyl groups upon suitable treatment with concentrated hydrochloric acid. The DP-MS samples obtained by using up to 20% of DPTS featured hexagonally ordered mesopores, narrow pore size distribution and high specific surface area. Conversion of DP-MS to mesoporous silica with hydroxyphosphatoethyl groups (POH-MS) resulted in the enlargement of the specific surface area, total porosity, and microporosity. High affinity of hydroxyphosphatoethyl groups toward lead ions (Pb(2+)) makes the POH-MS materials attractive sorbents for lead ions, which is reflected by high lead uptake reaching 272 mg of Pb(2+) per gram of POH-MS. This study shows that the simple and effective co-condensation strategy assures high loading of P-containing groups showing high affinity toward lead ions, which is of great importance for removal of highly toxic lead ions from contaminated water.
No takes yet. Share an insight, caveat, or question.
Gunathilake et al. (2015) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: