Answers are grounded in this paper and cite their sources.
We report details about the quantitative analysis of B and P impurities in the concentration range between 1 × 1014 and 1 × 1017 cm–3 by photoluminescence (PL) in solar‐grade Si (SOG‐Si). The intensity ratio of impurity‐bound exciton (BE) to free exciton (FE) at 4.2 K was used as a measure of the impurity concentration in the range between 5 × 1010 and 1 × 1015 cm–3 in the standard PL method. We raised the sample temperature to enhance the FE emission, which enabled us to extend the concentration range higher. The sample temperature was accurately determined from the FE‐line shape. We deduced a formula for the determination of the B and P concentrations in the higher range from the BE/FE ratio and the sample temperature (© 2011 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)
No takes yet. Share an insight, caveat, or question.
Iwai et al. (2010) studied this question.
Synapse has enriched 5 related papers. Consider them for comparative context: