Thermal oxidation produced cu2o from copper foils at 1020°C, suggesting potential for material enhancement.
Cu 2 O has been obtained via the thermal oxidation of free-standing Cu foils with a thickness of 127 μm under Ar and O 2 at 1020°C followed by controlled cooldown at -...