Answers are grounded in this paper and cite their sources.
Analysis reveals improved fatigue characteristics with greater reduction in diameter of trip steel wire, indicating implications for performance under cyclic loading.
The phase composition, static and fatigue mechanical properties of austenitic-martensitic trip-steel VNS9-Sh (23Kh15N5AM3-Sh - 23Х15Н5АМ3-Ш) have been studied at various stages of cold drawing: from a diameter of 2.4 mm to a diameter of 0.36 mm, which corresponds to the total degree of reduction (accumulated strain) 31.5 and 86%, respectively. It was established that with an increase in the accumulated strain from 31.5 to 45%, the proportion of martensite in the bulk of the material increased from 15 to 20.4% at a comparable strength level (1800-1850 MPa), while the yield strength increased and the relative elongation decreased. With an identical phase composition (from 15 to 20.4% martensite in the volume and not more than 14% on the surface) and a comparable tensile strength (from 1800 to 1850 MPa), the fatigue characteristics of a wire with a diameter of 0.95 mm were higher than wires with a diameter of 2.4 mm.
No takes yet. Share an insight, caveat, or question.
Prosvirnin et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: