Answers are grounded in this paper and cite their sources.
Research demonstrates hardness variation in CeO2 surface layer from Ti-29Nb-13Ta-4.6Zr alloy, indicating optimal sputtering conditions.
The structure, morphology and hardness of the surface layer of CeO2 formed on a plate of Ti-29Nb-13Ta-4.6Zr alloy by magnetron sputtering at various process parameters have been studied. It was established that under the selected conditions, the CeO2 layer of stoichiometric composition was formed (fluorite lattice, space group Fm3m). A linear dependence of the thickness of the surface layer on the duration of spraying and an extreme dependence, passing through the maximum, on power were revealed. A decrease in the hardness of the CeO2 layer with increasing the thickness was noted. At small coating thicknesses (up to 720 nm), the formation of the TiO2 sublayer is observed.