This analysis shows how tempering temperature affects mechanical properties and corrosion resistance in low-carbon steel, suggesting limited tempering may suffice.
The effect of tempering temperature (300-600 °C) on the structure, mechanical properties and corrosion resistance of 05KhGB (05ХГБ) low-carbon steel with a lath-type bainite structure obtained by quenching from 880 or 920 °C has been studied. It is shown that low-carbon steel with a lath-like carbide-free bainite structure formed during accelerated cooling is characterized by a combination of high strength and increased ductility. The steel resistance to corrosion-mechanical fracture in oilfield environments does not change significantly with the tempering temperature, which makes possible to exclude the tempering operation from heat treatment or limit it to low-temperature tempering.
No takes yet. Share an insight, caveat, or question.
Vyboyshchik et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: