This investigation shows interfacial defects worsen bonding in multi-layer AFS structures, revealing critical insights into defect management.
Additive friction surfacing (AFS) deposition is a process used for developing large structural products, where multi-layer deposition is inherently required. Even using optimized parameters, fundamental process limitations lead to the formation of non-bonded edges and interfacial defects in multi-layer structures. However, product performance grossly depends on the presence of defects and, more crucially, their impact on interfacial bonding. Edge trimming and intermediate surface machining after each layer deposition can remove edge defects and interfacial defects to a certain extent. Thus, machining cannot be a viable solution for the complete removal of internal defects. This paper investigates the impact of defects in multilayer AFS-deposited structures by analyzing X-ray microcomputed tomography (μ–CT) images and correlating them with flexural and interlayer bonding properties. Detailed defect analysis revealed that stress concentration occurred at sharp edges, and their subsequent propagation significantly weakened interfacial bonding between layers. Additionally, insights into the deposition and defect formation mechanisms enabled effective mitigation of defects through friction stir processing (FSP). With the reduced defect volume and improved sphericity of residual defects achieved through the FSP operation, the fabricated structures demonstrated 43.93 % higher flexural strength and no interlayer delamination under extreme bending.
No takes yet. Share an insight, caveat, or question.
Karmakar et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: