Answers are grounded in this paper and cite their sources.
Observational analysis found varying push-out bond strengths in three root canal sealers, indicating material differences.
Introduction: The adhesion of sealers to dentin is a vital aspect of endodontic success. Epoxy resin-based sealers such as AH Plus ® are considered the gold standard for their strong mechanical adhesion, but they lack bioactivity. Calcium silicate-based sealers such as AH Plus ® Bioceramic and Ceraseal ® offer bioactive potential. This study compares the push-out bond strength and failure modes of three root canal sealers: AH Plus ® Bioceramic, Ceraseal ® , and AH Plus ® . Materials and Methods: Thirty mandibular premolars were prepared and divided into three groups (n = 10): Group I (AH Plus ® Bioceramic), Group II (Ceraseal ® ), and Group III (AH Plus ® ). Push-out bond strength was measured in MPa at apical and medial root segments using a universal testing machine. Failure modes were evaluated using a digital microscope at ×30 and ×100 magnification. Results: AH Plus ® exhibited the highest mean bond strength (14.65 ± 2.42 MPa), followed by Ceraseal ® . AH Plus ® Bioceramic showed the lowest bond strength (2.31 ± 0.21 MPa). Failure modes in Group I were predominantly mixed, whereas Groups II and III had balanced cohesive and mixed failures. Conclusions: While all sealers adhered well to dentin, AH Plus ® Bioceramic demonstrated significantly lower bond strength compared to AH Plus ® and Ceraseal ® .
No takes yet. Share an insight, caveat, or question.
Maharti et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: