Answers are grounded in this paper and cite their sources.
The study demonstrates optimal ratios for ester synthesis and evaluates its thermal and chemical properties.
An ester based on polyglycidyl acrylate and ethylenediamine has been obtained, the structure of which has been confirmed by IR spectroscopy. It has been established that the molar ratio of diamine to polyglycidyl acrylate equal to 0.036:1 is optimal, at which the diamine is uniformly distributed in the polymer matrix. The obtained ester based on polyglycidyl acrylate and ethylenediamine does not interact with most organic solvents and is resistant to pH in the range of 6-11. It has been shown that the process of thermal destruction of the ester based on polyglycidyl acrylate and ethylenediamine occurs in two stages, and the mass loss at a temperature of 900 ºС is 86%. The activation energy of the decomposition reaction of the ester based on polyglycidyl acrylate and ethylenediamine is 70.3 kJ/mol. The obtained ester based on polyglycidyl acrylate and ethylenediamine has been tested as a coating for a steel metal surface. It was found that in aqueous solutions, the hydrophobic properties of polymer coatings deteriorate at a pH of the medium from 2 to 4, which is associated with the hydrophilization of the surface as a result of chemical interaction due to the hydration of active centers capable of forming hydrogen bonds with unused epoxy and ester monomer groups of polyglycidyl acrylate, which leads to a sharp swelling of the polymers
No takes yet. Share an insight, caveat, or question.
Липин et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: