Experimental investigation improves synthetic oil yield in kerogen-rich shale using iron nitrate catalyst.
The effectiveness of an iron nitrate catalyst (Fe(NO3)3·9H2O) was experimentally investigates to improve the efficiency of steam injection for in-situ hydrothermal conversion of Domanik low-permeable shale rock, with the aim of improving both the quantity and quality of produced synthetic oil. The experiments were performed under hydrothermal condition at 300℃ and 350℃ for 24 hours and at 400℃ for 3 hours. The generated synthetic oils and produced gases was analyzed using GC, GC-MS chromatography, gas chromatography, elemental and SARA analysis. The obtained results revealed that the addition of iron nitrate led to a significant increase in synthetic oil yield by 2.56% at 300℃, 5.39% at 350℃ and 4.87% at 400℃, as opposed to non-catalytic conditions. The optimal condition was identified at 350℃, which yielded higher amounts of light n-alkanes (C9-C20) compared to heavy n-alkanes. The results of SARA analysis and GC-MS also showed high aliphatic hydrocarbons content within the generated synthetic oil. Furthermore, XRD analysis revealed that the presence of iron sulfides (FeS2) and iron oxides (Fe2O3) plays a significant role in facilitating the effective desulfurization of bitumen and kerogen. These findings highlight the catalytic potential of water-soluble iron nitrate in hydrothermal treatment, offering valuable insights for optimizing synthetic oil production from oil shale.
No takes yet. Share an insight, caveat, or question.
Saeed et al. (2025) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: