Experiment assesses FGD gypsum with calcium aluminate cement reducing shrinkage in alkali-activated mortars, suggesting potential for industrial waste valorization.
Mineral expansive from FDG—flue-gas desulfurization—blended with calcium aluminate cement CAC was analyzed as mitigation shrinkage of alkali-activated residual mortars AAM. The AAM mortars were composed of red mud (RM) and bottom ash (BA), as precursors of a metakaolin MK-based system. MK replacement (0, 50, 70%) in alkaline solution (10M) and ratio 1:2 (binder/sand) was studied. Engineering properties were performed, and included mechanical strength, setting times, and dry shrinkage (HR 60%), as well as the microstructure formed at 7 d and 28 days. A total of 10% CAC-FGD dosage was the most efficient, reducing drying shrinkage by 23% and autogenous shrinkage by up to 30%. The findings showed that this addition also improved mechanical strength by approximately 16% at 28 days. Under the addition of CAC-FGD, the results suggest the presence of aluminosilicate gels of the (Na,C)-(A)-S-H type and the formation of ettringite, which are possibly responsible for ensuring good performance and a controlled expansion that, in turn, compensates for the shrinkage of the activated mortars.
No takes yet. Share an insight, caveat, or question.
Moura et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: