As a key component for wearable electronics, intrinsically stretchable and healable semiconducting polymers are scarce because carrier mobility is often reduced with increasing stretchability and self-healability. Here, we combine stepwise polymerization and thermal conversion to introduce in situ continuous hydrogen bonding sites in a polymer backbone without breaking the conjugation or introducing bulky softer side chains, benefiting the intrachain and interchain charge transport. We demonstrate that a regular sequence structure facilitated the formation of big nanofibers with a high degree of aggregation, providing the loose and porous thin film with simultaneously improved charge transport, stretchability, and self-healability. The mobility of damaged devices can be recovered to 81% after a healing treatment. Fully stretchable transistor based on the designed polymer exhibited a greatly enhanced mobility up to 1.08 square centimeters per volt per second under 100% strain, which is an unprecedented value and constitutes a major step for the development of intrinsically stretchable and healable semiconducting polymers.
No takes yet. Share an insight, caveat, or question.
Yue et al. (2024) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: