Luminescent solar concentrators (LSCs) were made by the infiltration of microfibrous thin films (µFTFs) of Parylene C by Lumogen F Red 305 (LFR305), in order to maximize the concentration of light made available to a photovoltaic solar cell (PVSC). The Parylene-C µFTFs with either tilted columnar or chevronic morphology were fabricated using physicochemical vapor deposition and infiltrated with LFR305 using thermal evaporation. Application of a voltage across a photoresistor illuminated by a solar simulator (AM1.5) through a LFR305-infiltrated Parylene-C LSC resulted in an enhancement of the ON-OFF minimum current ratio by a factor of 1.5 ± 0.29 compared to the ratio before LFR305 infiltration/deposition, regardless of morphology; furthermore, LFR305 infiltration enhanced the ON-OFF minimum current ratio by 56.5 ± 21.5%, depending on the morphology. The LSC concentration factor was determined to be 8.0 ± 3.1 after integration with a monocrystalline-silicon solar cell, depending on the morphology.
No takes yet. Share an insight, caveat, or question.
Li et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: