Tungsten (W) samples containing 0, 1, 3, and 5 at.% rhenium (Re) were irradiated by 20 MeV W ions to 0.5 dpa at 290 K and to 0.3 dpa at 1350 K. An additional set of samples was irradiated to 0.5 dpa at 290 K and then annealed at 1350 K. The irradiated samples were exposed to a deuterium (D) plasma at 370 K. D concentration profiles in the samples were measured using the D(He3,p)α nuclear reaction analysis. The D binding states in the defects were analysed using thermal desorption spectroscopy (TDS). In the case of irradiation at 290 K, the trapped D concentration monotonically increases with increasing Re concentration: in W-5%Re it is 17 % higher than in pure W. On the contrary, for irradiation at 1350 K the trapped D concentration monotonically decreases with increasing Re concentration: in W-5%Re it is 50 times smaller than in pure W. In the case of annealing at 1350 K of the samples irradiated at 290 K, the Re presence yields only up to three times reduction of trapped D concentration compared with pure W. TDS shows that the nature of D trapping sites is different for the irradiations at 290 K and 1350 K. We attribute the reduced D trapping in W-Re alloys irradiated at 1350 K to the reduction of cavity growth caused by the presence of Re.
No takes yet. Share an insight, caveat, or question.
Zibrov et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: