Abstract Induction solution heat treatment can change the mechanical characteristics and corrosion resistance properties of 308L manufactured via wire arc additive manufacturing (WAAM). Moreover, compare with traditional heat treatment methods, this method can reduce heat treatment time and achieve in-situ local heat treatment. By applying induction solution heat treatment to 308L fabricated using WAAM, ferrite and austenite phase proportions were changed. Heat treatment at 1100 ℃ effectively reduced the δ-Fe and σ-Fe content, resulting in a slight decrease in UTS, while YS, EL, and microhardness have a certain degree of increase. σ-Fe exhibits a more pronounced strengthening effect than austenite, albeit at the potential expense of steel's elasticity. At the same time, induction heat treatment alters the ferrite to austenite ratio, which also enhances the anti-corrosion properties of the stainless steel. However, the presence of σ-Fe will cause a worsening of the corrosion resistance of the steel. In addition, as the heat treatment progress advances, there is a notable transformation in the ferrite's microstructure in the deposition direction, from continuous dendrites to a small number of equiaxed grains.
No takes yet. Share an insight, caveat, or question.
Sun et al. (2024) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: