Mg-Ca-Zn-Mn alloys are promising for applications in biodegradable bone fixation devices. The Zn/Ca atomic ratio in the compositions of these alloys is important to their corrosion and mechanical properties. This paper investigated the Zn/Ca ratio using a phase-focused approach based on CALPHAD (CALculation of PHAse Diagrams) modeling and experimental validation. Six Mg-0.5Ca-xZn-0.5Mn (all wt.%) alloys were cast with x = 0.96, 1.15, 1.47, 1.69, 1.94, and 3.81 so that the Zn/Ca atomic ratio spanned from 1.18 to 4.66. The microstructure is studied in the as-cast, solution-treated, and as-rolled conditions. A critical ratio was determined to be 2.77, above which Mg2Ca phase can be suppressed in as-cast microstructure. In the solution-treated condition, a Zn/Ca ratio of less than 2.0 was required to dissolve the Ca2Mg6Zn3 phase. Alloys below 2.0 Zn/Ca were found to have yield strength of 300 MPa and a corrosion rate of 0.25 to 0.3 mg/cm2/day as measured by both weight loss and hydrogen evolution. In alloys above 2.0 Zn/Ca, the yield strength decreased to 280 MPa and the corrosion rate measured by weight-loss increased to 0.5 mg/cm2/day. Above the critical ratio, the yield strength was the highest at 347 MPa but a corrosion rate of 0.4 mg/cm2/day. The Zn/Ca region with the best combination of corrosion resistance and mechanical properties is between 1.18 and 1.8 (in rolled sheet condition), which provides important guidance for biomedical Mg-Ca-Zn alloy design and optimization.
No takes yet. Share an insight, caveat, or question.
Avey et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: