Al L B 14 ( L =Li or Na or K) crystals were grown using LiF or NaF or KF and crystalline boron powders as the starting materials using a high-temperature Al melt at soaking temperature 1573 ∼ 1773 K for a soaking time of 5 h under an Ar atmosphere. AlLiB 14 and AlNaB 14 crystals were obtained from LiF or NaF and B powders, and the atomic ratios ( n =B/ L = 2.0 ∼ 4.0) of starting materials. The AlKB 14 crystal was not obtained from KF and B powders as starting materials. The micro-Vickers hardness of Al L B 14 crystals is 24(±1) GPa for AlLiB 14 and 25(±1) GPa for AlNaB 14 . The oxidation initiation temperature of AlLiB 14 was about 815 K, and the peak due to the exothermic reaction was about 960 K for AlLiB 14 and about 990 K for AlNaB 14 . The final oxidation products were Li 2 B 2 O 4 , Al 4 B 2 O 9 , B 2 O 3 , and amorphous phases. The values for the electrical resistivity of the Al L B 14 compound were 2.4 ∼ 157 Ω·cm.
No takes yet. Share an insight, caveat, or question.
Hagiwara et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: