The study investigates salt chemistry and corrosion behavior of SS 316H and Alloy 617 in thermally purified molten NaF‐KF‐UF 4 ‐UF 3 salts (UF 4 /UF 3 initial ratio 12–14) at 800°C for 120, 72, and 32 h. UF 4 /UF 3 ratio increases after corrosion tests. Cr species concentration in salts keeps increasing. Fe, Co, Ni, and Mo species increase first, then decrease. Cr/Mn oxides are formed along grain boundaries in SS 316H. Cr near the surface of Alloy 617 is completely depleted. A thin layer composed of Fe, Co, Ni, and Mo is observed on the Alloy 617 surface in 72‐h and 32‐h tests.