Answers are grounded in this paper and cite their sources.
The use of wood powder can be reduced by a mixture of cinnamon, bamboo powder, and steel wool as a filling of the composite particle board. The length of steel wool in this study was determined by the size, i.e. 2, 4, and 6 mm. The composite composition comparison was 30% cinnamon powder, 30% bamboo Powder, 1% wool steel, 29% PVAc, and 10% epoxy resin. Compression process using the cold press single punch method for 2 hours then post curing process at a temperature of 150 oC for 1 hour. The results of this study show that steel wool length influences the characteristics of the particle board, both physical properties, mechanical properties, and morphological structure.
No takes yet. Share an insight, caveat, or question.
Ramadhan et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: