In this study, a novel composite solder, Sn-3.5Ag-10.0Co, was tailored for transient liquid phase (TLP) bonding in electric vehicle power module integration. Employing a meticulous two-step joining process, the solder joint was transformed into a robust microstructure characterized by two high-melting point intermetallic compounds, Ni3Sn4 and (Co,Ni)Sn2. After 1 h of TLP bonding, the Sn-3.5Ag-10.0Co paste transformed into the IMCs, but voids persisted between them, particularly between (Co,Ni)Sn2 and Ni3Sn4. Voids significantly reduced after 2 h of bonding, with full coalescence of the joint microstructure observed. The joint continued to be densified after 3 h of TLP bonding, but voids tended to accumulate at the joint center. Failure analysis revealed crack propagation through Ni3Sn4/(Co,Ni)Sn2 interfaces and internal voids. The engineered Sn-Ag-Co TLP joint exhibited superior shear strength retention even at an elevated temperature of 200 °C, contrasting with the significant reduction observed in the Sn-3.5Ag control specimen due to remaining Sn.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: