A processing scheme for preparing strips of Al−Cu−Li−Mg−Zr-based alloys microalloyed with Sc was proposed. This scheme includes a twin-roll casting of strips with a near-net-shaped 3 mm-thick gauge and a homogenization/solution treatment processing step. Two twin-roll cast Al−Cu−Li−Mg−Zr-based alloys were studied, one with an addition of 0.17 wt.% Sc, and the other without addition of Sc. Both alloys were annealed at 300 °C for 30 min, 450 °C for 30 min, and 530 °C for 30 min and quenched into room temperature water. The first two annealing steps provide a fine dispersion of Al3Zr/Al3(Sc,Zr) particles. The final annealing step serves as homogenization/solution treatment. A fine crystallization structure of the twin-roll cast materials enables the dissolution of primary particles containing the main alloying elements during a relatively short annealing time. Shorter soaking duration limits the depletion of surface layers from Li and significant coarsening of Al3Zr/Al3(Sc,Zr) dispersoids. The Sc-containing material has significantly finer grains already in the as-cast state. The Al3(Sc,Zr) dispersoids formed during the homogenization/solution treatment step prevent grain coarsening at high temperatures. Strengthening θ′(Al2Cu), T1(Al2CuLi), and rare S'(Al2CuMg) phases are formed during subsequent artificial aging at 180 °C. The increase in yield strength was 200 MPa in the peak-aged conditions. This value is comparable to the ones reported in similar direct-chill cast materials, thus validating the proposed processing scheme.
No takes yet. Share an insight, caveat, or question.
Králík et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: