Pitting corrosion is harmful and often occurs in chloride solution. The pitting corrosion of 4Cr13 steel in a chlorine tank was investigated in this study. Cr-depleted rings were observed and the Cr-depleted ring coincided with the bumps consisting of corrosion product. Carbides distributed along the Cr-depleted ring were also observed. Many pitting with spherical or shallow shapes were observed by cross-section morphology exam. The depth of pitting for Sample A is smaller than that for Sample B which accorded with surface morphology. The corrosion product was composed of a Fe-rich outer layer and a Cr-rich inner layer. The Fe-rich outer layer will rapture and fall off with the increase of corrosion products, and then the Cr-rich inner layer was revealed. As a result, Cr-depleted rings were inspected with SEM-EDS. The pitting corrosion mechanism of 4Cr13 steel in the chlorine tank was also discussed.
No takes yet. Share an insight, caveat, or question.
Li et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: