Addressing critical challenges in enhancing the oxidative stability and proton conductivity of high-temperature proton exchange membranes (HT-PEMs) is pivotal for their commercial viability. This study uncovers the significant capacity of multiwalled carbon nanotubes (MWNTs) to absorb a substantial amount of phosphoric acid (PA). The investigation focuses on incorporating long-range ordered hollow MWNTs into self-cross-linked fluorenone-containing polybenzimidazole (FPBI) membranes. The absorbed PA within MWNTs and FPBI forms dense PA networks within the membrane, effectively enhancing the proton conductivity. Moreover, the exceptional inertness of MWNTs plays a vital role in reinforcing the oxidation resistance of the composite membranes. The proton conductivity of the 1.5% CNT-FPBI membrane is measured at 0.0817 S cm–1 at 160 °C. Under anhydrous conditions at the same temperature, the power density of the 1.5% CNT-FPBI membrane reaches 831.3 mW cm–2. Notably, the power density remains stable even after 200 h of oxidation testing and 250 h of operational stability in a single cell. The achieved power density and long-term stability of the 1.5% CNT-FPBI membrane surpass the recently reported results. This study introduces a straightforward approach for the systematic design of high-performance and robust composite HT-PEMs for fuel cells.
No takes yet. Share an insight, caveat, or question.
Huang et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: