This is the authors' abstract. We don't add key points for this paper.
Structural modifications of single-walled aluminosilicate clay nanotubes have been studied under hydrostatic pressure by in situ synchrotron X-ray scattering. Imogolite nanotubes (INT) of nominal composition (OH)3Al2O3SiOH, and methyl-modified imogolite nanotubes (m-INT), (OH)3Al2O3SiCH3, have hydrophilic and hydrophobic internal cavities, respectively. Nanotube chiralities also differ, with zigzag (INT) and armchair (m-INT) chirality. In this work, pressure-induced changes in nanotube morphology and atomic structure are studied as a function of chirality, affinity of the inner cavity, and the pressure-transmitting medium used. Radial deformation and collapse of nanotubes are evidenced below 3 GPa, followed by the formation of a lamellar phase at higher pressures. In the case of INT, the collapse pressure value depends on the pressure transmitting medium chosen. Axial compressibility is measured, and a pseudo Young's modulus Y is determined to be equal to ∼265 GPa for INT and below 80 GPa for m-INT, underpinning the role of nanotube chirality in mechanical properties.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Rouzière et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: