Deposition models are being developed with the commercial computational fluid dynamics software STAR-CCM+ to evaluate particulate deposition on spent nuclear fuel (SNF) canisters. The primary particulate of concern is chloride salts, which are dispersed in the atmosphere and then deposited onto the canisters. During dry storage, the primary degradation process is likely to be chloride-induced stress corrosion cracking (CISCC) at the heat-affected zones of the canister welds. It is known that stainless steel canisters are susceptible to CISCC; however, the rate of chloride deposition onto the canisters is poorly known, based on sparse field data from a small number of sites.