To provide polyimide (PI) with high heat resistance and ultra-low coefficient of thermal expansion (CTE) for use in flexible display substrates, a novel diamine with bisbenzimidazole and bisamide groups, namely N,N'-(1H,1'H-[5,5'-bibenzo[d]imidazole]-2,2'-diyl)bis(4-aminobenzamide) (BZBA), was designed and successfully synthesized. Several poly(benzimidazole-amide-imide) (PBIAI) films were prepared by thermal imidization with 3,3',4,4'-biphenyltetracarboxylic dianhydride (BPDA), 4,4'-oxydiphthalic anhydride (ODPA), 3,3',4,4'-benzophenonetetracarboxylic dianhydride (BTDA), and 4,4'-(hexafluoroisopropylindene)-diphthalic anhydride (6FDA), respectively. Among them, BZBA-BPDA has a high glass transition temperatures ( T g = 345 °C) while achieving an extremely low coefficients of thermal expansion (CTE = 1.9 ppm K −1 ), meeting the processing requirements of polymer flexible substrates in OLED devices. The effects of different dianhydrides on the performance of PBIAIs were compared, providing a meaningful reference for further adjusting the PI molecular structure to meet specific requirements for industrial polymer films.
No takes yet. Share an insight, caveat, or question.
Fang et al. (2024) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: