Answers are grounded in this paper and cite their sources.
In this study, powders of the τ–Mn 53.3 Al 45 C 1.7 hard magnetic phase were mixed and sintered with powders of the three soft magnetic phases, Fe 58.5 Co 31.5 X 10 (X=Ti, Zr, and Ce), in a relation of 98/2 wt.%. The soft Fe 58.5 Co 31.5 X 10 magnetic phases primarily exhibit an α–FeCo crystalline phase. The Fe 58.5 Co 31.5 Zr 10 and Fe 58.5 Co 31.5 Ce 10 samples contain the FeCoZr and Ce 2 (Fe,Co) 17 phases, respectively. Mössbauer Spectroscopy analysis of the soft magnetic phases was carried out using sextets, and quadrupole splitting distributions. In addition, a small hyperfine field distribution was performed only for Fe 58.5 Co 31.5 Zr 10 . The majority sextet with a mean hyperfine field of 36.4 T was associated with the α–FeCo phase, and the most likely quadrupole splitting below 1.2 mm/s, were associated with Fe +3 , and those more significant than this value were associated with Fe +2 . The hysteresis loops confirm the soft magnetic behavior, with saturation magnetization values of approximately 150 Am 2 kg -1 . The τ–Mn 53.3 Al 45 C 1.7 phase reveals the presence of the τ (84 wt.%) and β (16 wt.%) crystalline phases, along with magnetic properties such as magnetization at 1.8 T of 38.2 Am 2 kg -1 , coercive field of 0.377 T, and maximum energy product of 3.6 kJm -3 . The mixtures of both phases exhibit the soft magnetic phase α–FeCo and τ and β phases of the Mn-Al-C system. Among the three obtained mixed and sintered samples obtained, the one mixed with Fe 58.5 Co 31.5 Zr 10 demonstrates the best magnetic properties, with magnetization reaching 58.1 Am 2 kg -1 , a coercive field of 0.361 T, and a maximum energy product of 7.4 kJm -3 . All of these magnetic properties surpass those of the τ–Mn 53.3 Al 45 C 1.7 phase, except for the coercive field.
No takes yet. Share an insight, caveat, or question.
Sánchez et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: