Answers are grounded in this paper and cite their sources.
Tb3+ doped BaAl2O4 phosphors (0–9.0 mol%) were prepared through sol–gel combustion method. The crystal structure, morphology, chemical composition, photoluminescence (PL), afterglow and thermoluminescence (TL) glow curve of Tb3+ doped BaAl2O4 were investigated by means of X-ray diffraction, scanning electron microscopy, transmission electron microscopy, energy dispersive X-ray spectroscopy, PL spectroscopy, afterglow spectroscopy, and TL dosimetry. Characterizations of the PL and afterglow spectra indicate that both Tb3+ doping species and oxygen vacancies act as the luminescence center of PL whereas only Tb3+ dopant works as the luminescence center of afterglow for Tb3+ doped BaAl2O4. The green afterglow of Tb3+ doped BaAl2O4 lasts for about 214 min at the optimal doping concentration of about 1.0 mol%. The profile of TL glow curve of Tb3+ doped BaAl2O4 heavily depends on the doping concentration, and the evolution of the TL glow curve with doping concentration reveals that doping BaAl2O4 with Tb3+ can significantly modify the distribution of carrier traps in the phosphor. The effects of Tb3+ doping on the PL, afterglow, and TL glow curve of Tb3+ doped BaAl2O4 are discussed in terms of the creation, recombination, and neutralization of defects in BaAl2O4. This work proves that doing with Tb3+ species is a general and robust strategy for endowing BaAl2O4 with highly efficient green afterglow. This "defect engineering" approach enables ultra-long afterglow for Tb3+ doped BaAl2O4 when defect centers in the phosphors are optimized.
No takes yet. Share an insight, caveat, or question.
Cai et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: