Answers are grounded in this paper and cite their sources.
FeCrAl alloy, a promising candidate for accident tolerance fuel (ATF) cladding, has relatively low resistance to general corrosion in high temperature water. To improve the corrosion resistance, a continuous Al2O3 layer was formed on the surface of FeCrAl alloy through gaseous pre-oxidation. It was found that such treatment can significantly improve its corrosion resistance in high temperature hydrogenated water. The thickness of inner oxide layer after exposure to 320°C hydrogenated water for 950 h was reduced by ∼40%. In addition, the size and density of outer oxide particles were also decreased. However, the Al2O3 film pre-formed on FeCrAl alloy had poor stability in high temperature water and its long-term effect needs to be further evaluated.
No takes yet. Share an insight, caveat, or question.
Xie et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: