The paper studies the influence of arc welding technological processes on the resistance of welded joints of sparcely-alloyed weathering 06g2BDP steel to cold and hot cracking and brittle and fatigue fracture.with the help of the Implant method and using the technological tekken sample, the conditions for cold cracking were evaluated and the methods of their elimination were recommended.It is shown that with the use of mechanized welding in shielding gases, solid-section and flux-cored wires provide high technological strength of welded joints in terms of hot cracking in a wide range of welding modes.On the other hand, when using coated electrodes, this range is narrowed, and at V def ≥ 20 mm/min, joints are prone to the formation of this defect.the results of studies on the evaluation of welded joint resistance to brittle fracture indicate high values of the stress intensity factor K Q for both the weld and HAZ metal.The endurance limit of T-joints when tested by cyclic loading was determined, which is [σ] -1 = 35 MPa.
No takes yet. Share an insight, caveat, or question.
Haivoronskyi et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: